Coated Superheater for a Waste-to-Energy Plant Under “Toughened Conditions”

The plasma spraying process used here enables full protection of the flat coil assembly, including bends, suspension elements, spacer bars and other exposed areas.

The most interesting feature, however, is not immediately visible: working closely with the customer, we tailored the coating to the specific load profile along each section of the coil:

  • The front tube rows are coated with a highly abrasion‑resistant nickel‑based alloy.
  • The rear, less heavily loaded rows are protected with a reduced coating thickness.
  • The front bend sections are given additional targeted protection.

 

By optimally matching the coating system to the thermal and mechanical loads, the service life of the superheater has been increased from 18 months to 5 years in all boilers – while at the same time optimising overall costs.